INJECTION
PROBLEMS |
SOLUTION |
INJECTION
PROBLEMS |
SOLUTION |
SURFACE MELT
FLOW LINE |
1.TOO HIGH MELTING POINT |
MOLD
STRIP
DIFFICULTY |
1.DECREASE INJECTION PRESSURE |
2.ADJUST INJECTION SPEED |
2.DECREASE HOLDING PRESSURE TIME |
3.ENLARGE INLET SIZE |
3.INCREASE COOLING TIME |
4.MATERIAL NOT DRY ENOUGH |
4.CHECK MOLD TEMP. |
5.INCREASE MOLD TEMP. |
5.MOLD SURFACE TOO SMOOTH |
6.CHANGE INLET POSITION |
6.USE MOLD RELEASE AGENT |
CONNECTION
LINE |
1.INCREASE INJECTION SPEED |
7.INCREASE SLOPE OF EJECTOR PIN |
2.ADJUST MELTING TEMP. |
8.CHECK RESIN SHIRNKAGE RATE AND
MOLD SPEC. |
3.ENLARGE INLET SIZE OR CHANGE
INLET POSITION |
NOZZLE
DRIPPING
MELTed
MATERIAL |
1.DECREASE MELTING TEMP. |
4.SET AIR HOLE |
2.DECREASE NOZZLE TEMP. |
5.REMOVE CONNECTION OF FRONT
COLD RESIN |
3.DECREASE BACK PRESSURE |
PRODUCT
INDENTATION |
1.DECREASE INJECTION TEMP. |
4.DELAY TIME OF STRIPPING GATE'S
COLD RESIN |
2.INCREASE HOLDING PRESSURE |
WARPAGE |
1.BALANCE MOLD TEMP. |
3.INCREASE INJECTION PRESSURE |
2.CHECK INJECTION PRESSURE |
4.DECREASE MELTING TEMP. |
3.DECREASE INJECTION SPEED |
5.CHECK LENGTH OF RESIN
MEASURMENT AREA |
4.CHANGE INLET POSITION |
6.DECREASE MOLD LOCKING
PRESSURE & INCREASE EXHAUST |
5.CHECK MOLD LOCKING PRESSURE |
RESIN
NOT FULL IN
THE MOLD |
1.INCREASE MATERIAL SUPPLY |
TOUGHNESS
NOT
ENOUGH |
1.MELTING TEMP. IS TOO LOW OR
TOO HIGH |
2.INCREASE INJECTION PRESSURE TIME |
2.MATERIAL NOT DRY ENOUGH |
3INCREASE MELTING TEMP. |
3.DECREASE RECYCLE MATERIAL RATIO |
4.ENLARGE MOLD GATE, SPRUE, INLET |
4.CHECK CONTAMINATION |
5.USE BIGGER INJECTION MACHINE |
5.MATERIAL REMAIN TOO LONG TIME
IN THE SCREW |
6.CHECK SCREW HEAD |
6.USE TOUGHNESS AGENT TO IMPROVE
PHYSICAL PROPERTY |
7.INCREASE MATERIAL M.F.I. |
SCREW
CANNOT
ROLL |
1.INCREASE MELTING TEMP. |
BURNED |
1.DECREASE INJECTION SPEED |
2.DECREASE BACK PRESSURE |
2.ADJUST MELTING TEMP. |
3.FILL UP PROPER GREASE |
3.SET AIR HOLE |
4.STOP MACHINE & CHECK IF ANY
FOREIGN STUFF |